Pipe & Fittings
Description
Each length of pipe shall be subjected to the hydrostatic test. Also, each pipe shall be examined by a non-destructive examination method in accordance to the required practices.
The different mechanical test requirements for pipes, namely, transverse or longitudinal tension test, flattening test, and hardness or bend test are presented.Both ends of each crate will indicate the order no., heat no., dimensions, weight and bundles or as requested.
Material & Manufacture
Pipe may be either hot finished or cold drawn with the finishing heat treatment noted below.
Heat Treatment
A / N+T
N+T / Q+T
N+T
Mechanical Tests Specified
Transverse or Longitudinal Tension Test and Flattening Test, Hardness Test, or Bend Test
For material heat treated in a batch-type furnace, tests shall be made on 5% of the pipe from each treated lot. For small lots, at least one pipe shall be tested.
For material heat treated by the continuous process, tests shall be made on a sufficient number of pipe to constitute 5% of the lot, but in no case less than 2 pipe.
Read More
Alloy steel pipe Manufacturer
Alloy pipes, Alloy pipe, ASTM A333 alloy pipe, ASTM A335 alloy pipe, ASTM A213 seamless tube, Seamless tube, Seamless pipes
Address: No. 273, Siping Road, Shanghai, 200081, China,
Shanghai, Shanghai
China, 200081
Tel: 0086-21-33780199
Fax: 0086-21-61851035